Hunan Hemway Steel Co., Ltd.
Inconel Alloy 718 is non-magnetic. It maintains good corrosion resistance and oxidation resistance and is used for parts requiring high resistance to creep and stress rupture up to 1300°F (704°C) and oxidation resistance up to 1800°F (982°C).
|
STANDARD |
WERKSTOFF NR. |
UNS |
|
Inconel 718 |
2.4668 |
N07718 |
|
Grade |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
|
Inconel 718 |
0.08 max |
0.35 max |
0.35 max |
0.015 max |
0.30 max |
- |
50.00 - 55.00 |
17.00 - 21.00 |
|
Ultimate Tensile Strength, psi |
.2% Yield Strength psi |
Elongation % |
Hardness Rockwell B |
|
135,000 |
70,000 |
45 |
100 |